17CrNi6-6 Alloy Steel 1.5918 Engineering Steels
OTAI SPECIAL STEEL is 17CrNi6-6 Alloy Steel stockholders and suppliers from China. we have more our 16 years experience in special steel supply. supply in 17CrNi6-6 Alloy Steel 1.5918 Engineering Steels round bar, plate, steel flat bar, square bar.
17CrNi6-6 alloy steel-structural, pressure vessel and engineering steel which is formulated for primary forming into wrought products. It has a moderately high density among EN wrought alloy steels. In addition, it has a moderately high electrical conductivity and a moderately high base cost.
Equivalent grades of steel 17CrNi6-6 Alloy Steel (1.5918)
DIN 1.5918
EN 17CrNi6-6
Form of Supply
17CrNi6-6 Alloy Steel (1.5918), we can supply the round bar, flat bar, plate and square block. Diameters can be sawn to your required lengths as one offs or multiple cut pieces. Rectangular pieces can be sawn from flat bar or plate to your specific sizes. Ground tool steel bar can be supplied, providing a quality precision finished bar to tight tolerances
Size&Tolerance&Process
Shape | Size(mm) | Process | Tolerance | Length(mm) |
Round | Φ6-Φ50 | Cold Drawn | H11 | 3000-5800 |
Round | Φ40-Φ300 | Hot Rolled | -0/+3mm | 3000-10000 |
Round | Φ120-Φ1000 | Hot Forged | -0/+3mm | 3000-10000 |
Flat/Square/Block | Thickness:120-800 Width:120-1500 |
Hot Forged | -0/+3mm | 500-6000 |
Chemical Composition(%) of 17CrNi6-6 Alloy Steel
C | Mn | Si | P | S | Cr | Ni |
0.14-0.20 | 0.50-0.80 | 0.40 max | 0.025 max | 0.035 max | 1.40-1.70 | 1.40-1.70 |
Heat treatment
Process | Temperature(oC) |
Forging or hot rolling | 1100-850 |
Normalizing | 850-880 |
Soft annealing | 650-700 |
Carburising | 880-980 |
Core hardening | 830-870 |
Intermediate annealing | 630-650 |
Case hardening | 780-820 |
Tempering | 150-200 |
Normalizing For 17CrNi6-6
1.Nominal normalizing temperature:850-880°C
2.Hold the temperature for several hours
3.Cooling in the air
Annealing For 17CrNi6-6
1.Nominal Annealing temperature:650-700°C
2.Cool slowly in the furnace
3.Maximum Brinell hardness of 229
Hardening and Tempering(QT) For 17CrNi6-6
1.Nominal Hardening temperature:820-870°C
2.Hold at this temperature then quench in oil or water
3.Tempering as soon as possible when the temperature low to ambient
4.Heat uniformly to a suitable temperature.
5.keep the material out of the furnace, then cool in the air
Mechanical Property
1.Tensile strength: 900-1100MPa
2.Yield point: 635MPa
3.Percentage reduction of area after fracture: 40%
4.Elongation after fracture: 11%
5.Impact test (+20°C): Longitud – 40~60J
Application
Alloyed case hardening steel for highly strained parts and good toughness at core tensile strength of 900 – 1200 N/mm². Driving bevel gears, crown wheels, gears, shafts, bolts for automotive and gear components.